Injection 1015GU6
| Characteristic | Unit | Test method | Measured value | |
|---|---|---|---|---|
| Mechanical property | ||||
| Tensile strength | MPa | ISO 527-1,2 | 185 | |
| Tensile strain at break | % | 4 | ||
| Tensile modulus | MPa | 9300 | ||
| Flexural strength | MPa | ISO 178 | 280 | |
| Flexural modulus | MPa | 8500 | ||
| Charpy notched impact strength | kJ/m2 | ISO 179-1/1eA | 14 | |
| Rockwell hardness | R.Scale | - | ISO 2039 | 120 |
| M.Scale | 100 | |||
| Thermal property | ||||
| Melting temperature | ℃ | ISO 11357 | 215~225 | |
| Temperature of deflection under load | 0.45 MPa | ℃ | ISO 75-1,2 | 220 |
| 1.8 MPa | 205 | |||
| Other property | ||||
| Density | g/cm3 | ISO 1183 | 1.36 | |