| Mechanical property |
| Tensile strength |
MPa |
ISO 527-1,2 |
45 |
| Tensile strain at break |
% |
>35 |
| Tensile modulus |
MPa |
1800 |
| Flexural strength |
MPa |
ISO 178 |
70 |
| Flexural modulus |
MPa |
1700 |
| Charpy notched impact strength |
kJ/m2 |
ISO 179-1/1eA |
85 |
| Tensile strength after moisture absorption |
MPa |
ISO 527-1,2 |
28 |
| Tensile modulus after moisture absorption |
MPa |
900 |
| Tensile strain at break after moisture absorption |
% |
>50 |
| Flexural strength after moisture absorption |
MPa |
ISO 178 |
24 |
| Flexural modulus after moisture absorption |
MPa |
500 |
| Charpy notched impact strength after moisture absorption |
J/m |
ISO 179-1/1eA |
125 |
| Rockwell hardness |
R.Scale |
- |
ISO 2039 |
110 |
| M.Scale |
45 |
| R.Scale(After Moisture absorption) |
87 |
| M.Scale(After Moisture absorption) |
12 |
| Thermal property |
| Melting temperature |
℃ |
ISO 11357 |
215~225 |
| Temperature of deflection under load |
0.45 MPa |
℃ |
ISO 75-1,2 |
75 |
| 1.8 MPa |
55 |
| Coefficient of linear thermal expansion |
x10-5/K |
ISO 11359-2 |
10.0 |
| Other property |
| Density |
g/cm3 |
ISO 1183 |
1.07 |
| Water absorption |
equilibrium |
% |
UBE method |
2.2 |